Nombre Químico | Nomenclatura D1418 | Temperatura Min de servicio | Temperatura Max de servicio | Dureza | Resistencia a la tensión | Elongación min.% | Aceites | Ácidos | Intemperie | Abración | |
Hule natural | Poli-isopreno | NR | -20°C | 80°C | 40 85 Shore A | 1550 PSIA | 440 % | Malo | Bueno | Malo | Bueno |
Nitrilo uso Industrial | Acrilonitrilo Butadieno | NBR | -25°C | 105°C | 60 a 65 Shore A | 500 PSIA | 400% | Bueno | Regular | Regular | Regular |
Nitrilo grado sanitario | Acrilonitrilo Butadieno | NBR | -25°C | 130°C | 60 a 65 Shore A | 650 PSIA | 500% | Bueno | Regular | Regular | Regular |
Silicón | Poli-Siloxano | SI | -60°C | 250°C | 40 a 85 Shore A | 650 PSIA | 300% | Regular | Regular | Excelente | malo |
Poliuretano | Poliesteruretano | PU | -40°C | 90°C | 55 a 60 Shore A | 280% a 400% | Bueno | Bueno | |||
Esponja de Silicón | Poli-Siloxano | SI | -50°C | 220°C | N/A | N/A | N/A | Regular | Malo | Excelente | Malo |
EPDM | Etileno Propileno | EPDM | -25°C | 140°C | 60 a 68 Shore A | 400/1050 PSIA | 500/550% | Malo | Bueno | Excelente | Regular |
Neopreno | Cloropreno | CR | -20°C | 130°C | 60 a 85 Shore A | 510/650 PSIA | 420%/500% | Bueno | Bueno | Bueno | Bueno |
Vitón | Fluoroelastomero | FKM | -50°C | 240°C | 70 a 75 Shore A | 750 PSIA | 340% | Excelente | Excelente | Excelente | Regular |